Industry News
-
Custom JF-2E Glass Measurement Workflow: Define the Change
A custom glass-measurement project becomes easier to define when the team can name the existing measurement task and the part of the workflow that prevents a useful result. JF-2E uses the optical waveguide effect to measure surface stress in chemically tempered and thermally tempered glass. The m...Read more -
JF-1A Solar-Glass Surface Stress Inspection Before Assembly
A solar-glass stress check is most useful when the quality team can identify the treatment, reach the intended surface and connect the observation to a specific lot decision. JF-1A is applied to measuring surface stress of thermally toughened and heat-strengthened glass. The measurement range is ...Read more -
AEM-01 Calibration and Edge-Stress Verification Guide
For a glass quality team, a changed edge-stress reading raises two questions: did the specimen change, or did the measurement conditions change? AEM-01 uses the photoelastic principle for non-destructive glass edge-stress measurement. Resolution is 1 nm or 0.1 MPa. A useful calibration and verifi...Read more -
OWADMS-01 Lab Versus Production Station Evaluation
A windshield optical project becomes harder to specify when the station location is chosen before the measurement task. OWADMS-01 automatically measures optical angular deviation, binocular deviation, and optical wedge angle. The measurement range is 70 arcmin or 4200 arcsec. The useful first dec...Read more -
JF-6 Calibration and Method Verification Planning
A chemical-strengthening laboratory needs to know whether a changing stress profile comes from the glass or from the measurement process. JF-6 uses scattered light photoelasticity to measure the stress distribution of chemically tempered glass. The stated stress range is CS 0~2000 MPa. Method ver...Read more -
JF-2E Thermal Tempered Glass Stress Measurement
A portable stress meter is useful only when its measurement route matches the glass. JF-2E uses the optical waveguide effect to measure surface stress in chemically tempered and thermally tempered glass. JF-2E is a portable version with a 3.5-inch PDA and a 4000 mAh battery. For a laboratory comp...Read more -
JF-1A Surface Stress Checks for Glass Furnace Setup
A furnace setup trial needs evidence from the glass it produces. JF-1A is applied to measuring surface stress of thermally toughened and heat-strengthened glass. The measurement range is 15~400 MPa. For a process engineer comparing trial runs, it provides a portable route to a defined surface-str...Read more -
AEM-01 Edge Stress Checks Before Destructive Verification
A glass investigation can lose useful evidence when the first action destroys the specimen. AEM-01 uses the photoelastic principle for non-destructive glass edge-stress measurement. Measurement length is 50 mm. That makes a defined edge segment available for examination while the sample is still ...Read more -
OWADMS-01 Wedge Evaluation for Laminated Windshields
In a laminated-windshield development program, evaluate the optical behavior of the finished glass alongside the interlayer specification. OWADMS-01 automatically measures optical angular deviation, binocular deviation, and optical wedge angle. The system measures optical wedge angle in the HUD a...Read more -
JF-6 Standard or Custom: Scope Your Measurement Project
Start a JF-6 purchase by defining the stress-depth task, then separate the requirements that change the sample interface or workflow. JF-6 uses scattered light photoelasticity to measure the stress distribution of chemically tempered glass. The stated stress range is CS 0~2000 MPa. It is a candid...Read more -
JF-2E Stress Checks for Smartphone Cover Glass
A cover-glass development team needs to understand both the surface-stress condition and the strengthened layer before comparing process candidates. JF-2E uses the optical waveguide effect to measure surface stress in chemically tempered and thermally tempered glass. The measurement range is 1000...Read more -
JF-1A Operator Training for Consistent Stress Readings
When two operators obtain different glass-stress readings, start by comparing how they measured the same sample at the same location. JF-1A is applied to measuring surface stress of thermally toughened and heat-strengthened glass. The measurement range is 15~400 MPa. It gives a glass-processing l...Read more